In 2008, after nearly a year of hard work, the research personnel has finally successfully trial-manufacture Liguang FRP plate and U-Gutter FRP, V-Gutter FRP and ridge tile FRP, to further improve the whole products' system of FRP composites.

The main detection indicators of Liguang FRP

Relative density

1.40-1.45

Glass fiber content

25-30(%)

Tensile strength

70-100(MPa)

Tensile elastic modulus

5000-7000(MPa)

Bending strength

200-250(MPa)

Bending elastic modulus

5000-7000(MPa)

Compressive strength

130-180(MPa)

Shear strength

70-100(MPa)

Elongation

1.0-1.5(%)

expansion coefficient

2.5(10-5/℃)

Impact strength(Bob)

12-13(J/m2)

Barcol hardness

M-70-M-120

Heat capacity

1.255[kJ/(kg.℃)]

Thermal conductivity

0.3-0.2[kcal/(m.h.℃)]

Water absorption

0.1-0.2[(24h)/%]

Heat-resistant temp

-120-160(℃)

Full-light transmittance

85%(1.5mm thick,colorless)

All-UV light transmittance

5%(1.5mm thick,colorless)